Navigation
|
A15: Fe, Cu, K, Al, Sr, Zn
Submitted by CSULA_Mark on Wed, 09/28/2011 - 13:01
Metals: Al, Cu, Fe, K, Sr, Zn
Electrolyte pH: Basic Comments: All chemicals began as 0.35 M of Metal Nitrate, 0.6M Ammonium Nitrate, and 0.015M HNO3 A15 Iron Copper Potassium Aluminum Strontium Zinc 1 = (row 1, col 1) Please feel free to retest these chemicals to confirm their consistency. Positive Bias - +0.07V Copper standard to the far right Baking Period: 5hrs 500C The Iron standard did not appear.
|
||||||||