Navigation
|
A25: Fe, Cu, Bi, K
Submitted by CSULA_Mark on Thu, 01/12/2012 - 16:12
Metals: Bi, Cu, Fe, K, Zn
Electrolyte pH: Basic Comments: All chemicals began as 0.35 M of Metal Nitrate, 0.6M Ammonium Nitrate, and 0.015M HNO3 0.15M Bismuth Nitrate, 1.45-1.58M of Nitric Acid added to solution, 0.6M NH4NO3 DI Filter to create the Bismuth Nitrate and Sodium Hydroxide solution had less than 1MΩ resistivity. A filter with resistivity greater than 1MΩ may provide cleaner results. A25 Iron Copper Bismuth Potassium Zinc 1 = (row 1, col 1) Hot Spots: Please feel free to retest these chemicals to confirm their consistency. Positive Bias - +0.07V Copper standard to the far right Baking Period: 5hrs
|
||||||||